A Transparent, Self-Healing, Highly Stretchable Ionic Conductor

Self-healing materials can repair damage caused by mechanical wear, thereby extending lifetime of devices. Here, a transparent, self-healing, highly stretchable ionic conductor is presented that autonomously heals after experiencing severe mechanical damage.