Is energy conservation satisfied in the current deformation application schemes in molecular dynamic simulations?

In our recent paper, we examined the energy conservation for the current schemes of applying active deformation in molecular dynamics (MD) simulations. Specifically, two methods are examined. One is scaling the dimension of the simulation box and the atom positions via an affine transformation, suitable for the periodic system. The other is moving the rigid walls that interact with the atoms in the system, suitable for the non-periodic system.