A cohesive zone framework for environmentally assisted fatigue (code included)

Emilio Martínez Pañeda's picture

I hope some of you find this work interesting, the code with the cohesive zone model for fatigue can be downloaded as a user element (UEL) subroutine for Abaqus from

A cohesive zone framework for environmentally assisted fatigue

Susana del Busto, Covadonga Betegón, Emilio Martínez Pañeda

Engineering Fracture Mechanics (2017)

We present a compelling finite element framework to model hydrogen assisted fatigue by means of a hydrogen- and cycle-dependent cohesive zone formulation. The model builds upon: (i) appropriate environmental boundary conditions, (ii) a coupled mechanical and hydrogen diffusion response, driven by chemical potential gradients, (iii) a mechanical behavior characterized by finite deformation J2 plasticity, (iv) a phenomenological trapping model, (v) an irreversible cohesive zone formulation for fatigue, grounded on continuum damage mechanics, and (vi) a traction-separation law dependent on hydrogen coverage calculated from first principles. The computations show that the present scheme appropriately captures the main experimental trends; namely, the sensitivity of fatigue crack growth rates to the loading frequency and the environment. The role of yield strength, work hardening, and constraint conditions in enhancing crack growth rates as a function of the frequency is thoroughly investigated. The results reveal the need to incorporate additional sources of stress elevation, such as gradient-enhanced dislocation hardening, to attain a quantitative agreement with the experiments.


Jiakun Zhu's picture

Thank you for your generous sharing!

JDI's picture

Nice work!

Subscribe to Comments for "A cohesive zone framework for environmentally assisted fatigue (code included)"

Recent comments

More comments


Subscribe to Syndicate