Hi all!!!
Could anybody please give some examples of materials possessing cubic symmetry (these materials need three independent elastic material properties).
Thanking you,
- R. Chennamsetti
»
- ramdas chennamsetti's blog
- Log in or register to post comments
- 13329 reads
Comments
cubic crystals
In the book, Thin Film Materials, by Ben Freund and Subra Suresh, there is a table of elastic constants for cubic crystals, including face-centered cubic (e.g., Ag, Au, Cu), body-centered cubic (W, Ta, Cr), diamond cubic (C, Si, Ge), and compounds (GaAs, InP, and NaCl). They all have three independent elastic constants.
RH
More elastic constants
You can find a few more in
Atomic and Electronic Structure of Solids
By Efthimios Kaxiras.
See here .
-- Biswajit