<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xml:base="http://imechanica.org" xmlns:dc="http://purl.org/dc/elements/1.1/">
<channel>
 <title>iMechanica - ES 246 project: Plane Strain Extrusion - Slip-line Field Solution vs. FEM Solution - Comments</title>
 <link>http://imechanica.org/node/508</link>
 <description>Comments for &quot;ES 246 project: Plane Strain Extrusion - Slip-line Field Solution vs. FEM Solution&quot;</description>
 <language>en</language>
<item>
 <title>Another question about the sliplines</title>
 <link>http://imechanica.org/node/508#comment-1401</link>
 <description>&lt;p&gt;Hi,&lt;/p&gt;
&lt;p&gt;Thanks alot for your help.&lt;/p&gt;
&lt;p&gt;I need to figure out a slip surface. In order to firgure out the plastic flow of a model, with just solving the static problem. The slip field  ( or surface in  3d model) would help me figure out the slip filed.&lt;/p&gt;
&lt;p&gt;I have another question which is not connected directly. I need to build a 3D surface with directions parallel to this surface. Its equivilant to an isosurface but instead it has the directions or planes parallel to the overall planes at each point. Does abaqus have this functin?&lt;/p&gt;
&lt;p&gt;Thanx again for your help  &lt;/p&gt;
&lt;br class=&quot;clear&quot; /&gt;</description>
 <pubDate>Thu, 01 Mar 2007 14:16:25 -0500</pubDate>
 <dc:creator>george salib</dc:creator>
 <guid isPermaLink="false">comment 1401 at http://imechanica.org</guid>
</item>
<item>
 <title>Thanks  a lot, i will chekc it out</title>
 <link>http://imechanica.org/node/508#comment-1402</link>
 <description>&lt;p&gt;i will check it out&lt;/p&gt;
&lt;br class=&quot;clear&quot; /&gt;</description>
 <pubDate>Thu, 01 Mar 2007 14:05:38 -0500</pubDate>
 <dc:creator>george salib</dc:creator>
 <guid isPermaLink="false">comment 1402 at http://imechanica.org</guid>
</item>
<item>
 <title>with Ms. Lu&#039;s permission...</title>
 <link>http://imechanica.org/node/508#comment-1300</link>
 <description>&lt;p&gt; Can I propse Mr. Hosford&amp;#39;s book to draw a simple slf under compression test ? If your question is just draw a simple net, it will helpfull I think.&lt;/p&gt;
&lt;br class=&quot;clear&quot; /&gt;</description>
 <pubDate>Wed, 21 Feb 2007 16:33:37 -0500</pubDate>
 <dc:creator>Hasan Yumak</dc:creator>
 <guid isPermaLink="false">comment 1300 at http://imechanica.org</guid>
</item>
<item>
 <title>The slip line field is given by theoretical analysis</title>
 <link>http://imechanica.org/node/508#comment-1186</link>
 <description>&lt;p&gt;Actually slip line field is given by theoretical analysis. It is just an assistant to determine the stress field eventually. If you can figure out the stress field directly from FEM why do you insist to get the slip line field?&lt;/p&gt;
&lt;br class=&quot;clear&quot; /&gt;</description>
 <pubDate>Thu, 15 Feb 2007 19:35:05 -0500</pubDate>
 <dc:creator>Nanshu Lu</dc:creator>
 <guid isPermaLink="false">comment 1186 at http://imechanica.org</guid>
</item>
<item>
 <title>Thanx for your answer,  one more question</title>
 <link>http://imechanica.org/node/508#comment-1185</link>
 <description>&lt;p&gt;Thank you for your answer for my earlier question. &lt;/p&gt;
&lt;p&gt;How can i get the slip-line field from the stress filed solution?&lt;/p&gt;
&lt;br class=&quot;clear&quot; /&gt;</description>
 <pubDate>Thu, 15 Feb 2007 19:09:45 -0500</pubDate>
 <dc:creator>george salib</dc:creator>
 <guid isPermaLink="false">comment 1185 at http://imechanica.org</guid>
</item>
<item>
 <title>As far as I know</title>
 <link>http://imechanica.org/node/508#comment-1146</link>
 <description>&lt;p&gt;Because I also used rigid plasticity in my ABAQUS model I can not tell how accurate perfect plasticity can be used to simulate real metal forming process.&lt;/p&gt;
&lt;p&gt;One assumption of slip-line field theory is the perfect plasticity. &lt;/p&gt;
&lt;p&gt;&amp;nbsp;&lt;/p&gt;
&lt;br class=&quot;clear&quot; /&gt;</description>
 <pubDate>Tue, 13 Feb 2007 11:43:48 -0500</pubDate>
 <dc:creator>Nanshu Lu</dc:creator>
 <guid isPermaLink="false">comment 1146 at http://imechanica.org</guid>
</item>
<item>
 <title>non-perfect plasticity</title>
 <link>http://imechanica.org/node/508#comment-1072</link>
 <description>&lt;p&gt;How accurate is the perfect plasticity for metal forming?&lt;br /&gt;How is the slip-line defined for a non-perfect plasticity?&lt;/p&gt;
&lt;p&gt;&amp;#160;&lt;/p&gt;
&lt;br class=&quot;clear&quot; /&gt;</description>
 <pubDate>Thu, 08 Feb 2007 17:35:16 -0500</pubDate>
 <dc:creator>Henry Tan</dc:creator>
 <guid isPermaLink="false">comment 1072 at http://imechanica.org</guid>
</item>
<item>
 <title>I&#039;m not sure</title>
 <link>http://imechanica.org/node/508#comment-1070</link>
 <description>&lt;p&gt;Hi George, &lt;/p&gt;
&lt;p&gt;The slip line is given by theoretical analysis here and I don&amp;#39;t think ABAQUS can explicitly draw the slip lines for you. But with the given stress field maybe you&amp;#39;ll be able to figure out the slip line field manually. &lt;/p&gt;
&lt;br class=&quot;clear&quot; /&gt;</description>
 <pubDate>Thu, 08 Feb 2007 17:17:32 -0500</pubDate>
 <dc:creator>Nanshu Lu</dc:creator>
 <guid isPermaLink="false">comment 1070 at http://imechanica.org</guid>
</item>
<item>
 <title>can abaqus give out the slip lines?</title>
 <link>http://imechanica.org/node/508#comment-1061</link>
 <description>&lt;p&gt;Can abaqus give out the slip lines?&lt;/p&gt;
&lt;br class=&quot;clear&quot; /&gt;</description>
 <pubDate>Thu, 08 Feb 2007 15:09:05 -0500</pubDate>
 <dc:creator>george salib</dc:creator>
 <guid isPermaLink="false">comment 1061 at http://imechanica.org</guid>
</item>
<item>
 <title>It&#039;s very interesting to</title>
 <link>http://imechanica.org/node/508#comment-472</link>
 <description>&lt;p&gt;&lt;span&gt;It&amp;#39;s very interesting to compare the analytical results from slip-line field theory to the numerical solutions of FEM software. &lt;/span&gt;&lt;span&gt;A problem you may encounter in this project is the model&amp;#39;s material property. The slip-line field theory assumes a plastic-rigid material, which has an infinite Young&amp;#39;s modulus below the yield point and no hardening upon yielding. As Prof. Vlassak mentioned in class, the numerical model with plastic-rigid material may lead to divergence. One possible solution to this problem might be to approximate the plastic-rigid condition as high Young&amp;#39;s Modulus, reasonable yield stress, and very low hardening. &lt;/span&gt;&lt;span&gt;Moreover, large distortions of elements may occur in your numerical model. If so, you may consider the ALE option for adaptive remeshing in ABAQUS.&lt;/span&gt;&lt;/p&gt;
&lt;br class=&quot;clear&quot; /&gt;</description>
 <pubDate>Fri, 08 Dec 2006 14:57:34 -0500</pubDate>
 <dc:creator>Xuanhe Zhao</dc:creator>
 <guid isPermaLink="false">comment 472 at http://imechanica.org</guid>
</item>
<item>
 <title>It might also be interesting</title>
 <link>http://imechanica.org/node/508#comment-462</link>
 <description>&lt;p&gt;It might also be interesting to consider unsymmetrical extrusions with ABAQUS.  There is a paper by A.P. Green which proposes slip-line fields and extrusion pressures for unsymmetrical extrusion through a sqare die.  I don&amp;#39;t know how difficult it would be to move the extrusion opening on your ABAQUS model, but it would be neat to see how the results compare to Green&amp;#39;s work. &lt;/p&gt;
&lt;p&gt;&amp;nbsp;&lt;/p&gt;
&lt;p&gt;&lt;span&gt;  GREEN AP, &lt;a href=&quot;http://apps.isiknowledge.com.ezp1.harvard.edu/WoS/CIW.cgi?SID=C1lKLF@oHI9c76M62bB&amp;amp;Func=Abstract&amp;amp;doc=1/9&quot;&gt;ON &lt;strong&gt;UNSYMMETRICAL&lt;/strong&gt; &lt;strong&gt;EXTRUSION&lt;/strong&gt; IN PLANE STRAIN&lt;/a&gt;,      JOURNAL OF THE MECHANICS AND PHYSICS OF SOLIDS 3 (3): 189-196 1955&lt;/span&gt; &lt;/p&gt;
&lt;br class=&quot;clear&quot; /&gt;</description>
 <pubDate>Thu, 07 Dec 2006 18:10:32 -0500</pubDate>
 <dc:creator>Jenn Furstenau</dc:creator>
 <guid isPermaLink="false">comment 462 at http://imechanica.org</guid>
</item>
<item>
 <title>ES 246 project: Plane Strain Extrusion - Slip-line Field Solution vs. FEM Solution</title>
 <link>http://imechanica.org/node/508</link>
 <description>&lt;p&gt;Due to maturity of FEM package, slip-line field theory is not widely used these days. However, we shall keep in mind that slip-line field analysis can provide analytical solutions to a number of very difficult problem which may involve huge deformations or velocity discontinuities, e.g. many metal forming processes. To evaluate these two analytical and numerical methods for plasticity I will try a simple example, compare these two solutions and finally get into a conclusion of my own. &lt;/p&gt;
&lt;p&gt;Following figure shows an example of metal-forming process known as Plane Strain Extrusion (Hill). I will first use slip-line field analysis to show that the force on the punch is given by P=2k(π/3+1/2)H. And then use ABAQUS/CAE to find out the numerical relation of P(H). If time permits I may also use ABAQUS/Explicit to dynamic analysis.  &lt;/p&gt;
&lt;p&gt;&lt;img src=&quot;http://www.engin.brown.edu/courses/En222/Notes/sliplines/sliplines_files/image018.gif&quot; border=&quot;0&quot; alt=&quot;Plane Strain Extrusion&quot; title=&quot;Plane Strain Extrusion&quot; width=&quot;400&quot; height=&quot;240&quot; /&gt;&lt;/p&gt;
&lt;p&gt; Journal articles:&lt;/p&gt;
&lt;p class=&quot;MsoNormal&quot;&gt;[1] &lt;span&gt;KOBAYASHI S, &lt;/span&gt;&lt;span&gt;PLANE-STRAIN SLIP-LINE FIELDS FOR METAL-DEFORMATION PROCESSES, JOURNAL OF APPLIED MECHANICS-TRANSACTIONS OF THE ASME 50 (3): 702-702 1983&lt;/span&gt;&lt;/p&gt;
&lt;br class=&quot;clear&quot; /&gt;</description>
 <comments>http://imechanica.org/node/508#comments</comments>
 <category domain="http://imechanica.org/taxonomy/term/316">ES 246</category>
 <category domain="http://imechanica.org/taxonomy/term/177">Fall 2006</category>
 <category domain="http://imechanica.org/taxonomy/term/169">Plasticity</category>
 <category domain="http://imechanica.org/taxonomy/term/307">project</category>
 <enclosure url="http://imechanica.org/files/ppt for ES 246 (01.11.2007).ppt" length="1187840" type="application/vnd.ms-powerpoint" />
 <pubDate>Tue, 28 Nov 2006 18:30:34 -0500</pubDate>
 <dc:creator>Nanshu Lu</dc:creator>