Micromechanics-Based Structural Analysis (FEAMAC) and Multiscale Visualization within Abaqus/CAE Environment
A unified framework is presented that enables coupled multiscale analysis of composite structures and associated graphical pre and post processing within the Abaqus/CAE environment. The recently developed, free, Finite Element Analysis - Micromechanics Analysis Code (FEAMAC) software couples NASA's Micromechanics Analysis Code with Generalized Method of Cells (MAC/GMC) with Abaqus/Standard and /Explicit to perform micromechanics based FEA such that the nonlinear composite material response at each integration point is modeled at each increment by MAC/GMC. The Graphical User Interfaces (FEAMAC-Pre and FEAMAC-Post), developed through collaboration between SIMULIA Erie and NASA Glenn Research Center, enable users to employ a new FEAMAC module within Abaqus/CAE that provides access to the composite microscale. FEAMAC-Pre is used to define and store constituent material properties, set up and store composite repeating unit cells, and assign composite materials as sections with all data being stored within the CAE database. Likewise FEAMAC-Post enables multiscale field quantity visualization (contour plots, X-Y plots), with point and click access to the microscale (i.e., fiber and matrix fields).
Attachment | Size |
---|---|
micromechanics-based-structural-analysis-feamac-2010.pdf | 34.91 KB |
- SIMULIA's blog
- Log in or register to post comments
- 5354 reads
Recent comments