CONTINUUM MODELING OF INTERFACES IN POLYMER MATRIX COMPOSITES REINFORCED BY CARBON NANOTUBES
L. Y. JIANG, H. TAN, J. WU, Y. HUANG, K. -C. HWANG
Review Article, 2007, accepted by NANO
The interface behavior may significantly influence the mechanical properties of carbon nanotube (CNT)-reinforced composites due to the large interface area per unit volume at the composite. The modeling of CNT/polymer interfaces has been a challenge in the continuum modeling of CNTreinforced composites. This paper presents a review of recent progress to model the CNT/matrix interfaces via a cohesive law established from the van der Waals force. A simple, analytical cohesive
law is obtained from the interatomic potential, and is used to study the effect of CNT/matrix interfaces on the macroscopic properties of CNT-reinforced composites.
- Henry Tan's blog
- Login or register to post comments
- 2340 reads


Recent comments
1 day 18 hours ago
1 day 23 hours ago
3 days 52 min ago
3 days 3 hours ago
3 days 14 hours ago
3 days 19 hours ago
3 days 21 hours ago
4 days 9 hours ago
5 days 2 hours ago
5 days 13 hours ago