I have done flat plate tensile test experiment with plate having u notch at different angle to get mixed mode behaviour.The experiment shows the force variation F(30 DEG)>F(45 DEG)>F(0 DEG)>F(60 DEG) While fem elasto-plastic model made in abaqus shows F(0 DEG)>F(30 DEG)>F(45 DEG)>F(60 DEG).
Can anyone tell me why this contradiction is there between experiment and fem model.
»