A cable bending stick-slip analytical model

Single strand cable bending, stick-slip, analytical models require that a choice be made between two contact modes between adjacent wires: either radial (between layers) or lateral (between same layer wires). In most recent models (e.g. Papailiou’s) radial contact is selected. A “lateral contact” model has been presented by Panetti in 1944 and can be found in the proceedings of the Turin Royal Academy of Science. A translated version from Italian is proposed in the attached file.

Panetti_English.pdf1.49 MB