On Weingarten-Volterra defects

Amit Acharya's picture

Amit Acharya

The kinematic theory of Weingarten-Volterra line defects is revisited, both at small and finite deformations. Existing results are clarified and corrected as needed, and new results are obtained. The primary focus is to understand the relationship between the disclination strength and Burgers vector of deformations containing a Weingarten-Volterra defect corresponding to different cut-surfaces.

AttachmentSize
finite_def_weingarten.pdf556.31 KB