Modeling water absorption in cement-based composites with SAP additions

Dear all,

We have recently presented our work on modelling of water absorption in concrete containing SAP (superabsorbent polymers) at the Euro-C conference in Austria. You can access the full paper at: https://www.researchgate.net/publication/323667669_Modeling_water_absorp...

Regards