Combined experimental and numerical study on micro-cube indentation splitting test of cement paste

Our group has recently published a paper describing a new method for micromechanical testing of cement paste. The paper was published in "Engineering Fracture Mechanics". Full paper can be accessed at:https://www.researchgate.net/publication/324510125_Combined_experimental...