Towards understanding stochastic fracture performance of cement paste at micro length scale based on numerical simulation

Dear all,

We have recently published an article aiming to understand the stochastic nature of the fracture process in hydrated cement paste through use of numerical simulation. The article can be viewed here: https://www.researchgate.net/publication/326180288_Towards_understanding...