http://www.ae.utexas.edu/~ruihuang/papers/PRB1.pdf
An epitaxial thin film can undergo surface instability and break up into discrete islands. The stress field and the interface interaction have profound effects on the dynamics of surface evolution. In this work, we develop a nonlinear evolution equation with a second-order approximation for the stress field and a nonlinear wetting potential for the interface. The equation is solved numerically in both two-dimensional (2D) and three-dimensional (3D) configurations using a spectral method. The effects of stress and wetting are examined. It is found that the nonlinear stress field alone induces “blow-up” instability, leading to crack-like grooving in 2D and circular pit-like morphology in 3D. For thin films, the blow-up is suppressed by the wetting effect, leading to a thin wetting layer and an array of discrete islands. The dynamics of island formation and coarsening over a large area is well captured by the interplay of the nonlinear stress field and the wetting effect.
- Yaoyu Pang's blog
- Login or register to post comments
- 2920 reads


Recent comments
8 hours 51 min ago
10 hours 20 min ago
16 hours 43 min ago
19 hours 14 min ago
19 hours 39 min ago
21 hours 7 min ago
1 day 6 hours ago
1 day 13 hours ago
1 day 13 hours ago
3 days 19 hours ago