Viscoelastic Abaqus Analysis question please help
Submitted by hdayanan on Mon, 2009-07-06 02:49.
Hi Everyone,
I am new to thermal viscosity analysis, here is the data I have received.
DMA data which has Temp, Shear Storage Modules, Shear Loss Modules, Tan Delta, Calculated Modules, Temp was raised at 5 deg/Min
I want to do a thermal analysis where the part is heated upto 90 deg for 1 hr, returned to room temp and cooled 2 hours.
How can i simulate this in abaqus ..? I want to incorporate the Viscosity data from the DMA data. I also have received thermal conductivity, thermal expansion and specific heat data.
please help, I greatly appreciate it,
kind regards
nadia