We have combined the EAM and the SW and the TF potentials in one functional form. This functional form allows the modeling of metal covalent systems (M-Si,Ge,C,SiC) very efficiently allowing the study of large systems. The potential iscalled as the "Angular-dependent Embedded Atom Method".
»