I was a little bit surprised in the introduction of this new forum to see mention of elastic and plastic contacts but no specific mention of viscoelastic contacts.
In the era of commercially-available instruments for indentation testing, the examination of viscoelastic contact mechanics, both in the context of polymers and biological tissues, seems to have taken on new life. To a first approximation, for indentation testing in the time domain, the fundamental mechanics has not much advanced beyond a few classic papers of the 1960s: Lee and Radok, J. Appl. Mech. 27 (1960) 438 and Ting TCT, J. Appl. Mech. 88 (1966) 845. However, the implementation of techniques for analysis of experimental data has progressed substantially. With spherical indenters the use of linearly viscoelastic models for characterization of a material creep or relaxation function is straightforward. Recent experimental studies have confirmed this, while more lingering questions remain for sharp contacts including Berkovich pyramidal indenters (most commonly shipped with commercial indenters). Sharp contacts seem to give rise to nonlinearly viscoelastic responses. Other topics of recent interest include frequency-domain measurements and examination of oscillating contacts and adhesion. (Although not mentioned in the listing of KLJ's most-loved topics in contact mechanics, viscoelastic contact has been the subject of several recent KLJ publications!) The research in viscoelastic contact mechanics has been strong in recent years, but perhaps a challenge remains in the dissemination of information and approachable experimental techniques for use by non-experts.