Fri, 2010-08-20 21:35 - KennyNg
I'm currently working on modeling 3 phases composites material. However, I'm having hard time on finding the transverse modulus as it's different from analytical results. I've been using Mori-Tanaka approach to determine the stiffness moduli. Does anyone know how to obtain a correct values for the transverse moduli?
»
- KennyNg's blog
- Log in or register to post comments
- 5457 reads
Comments
If you use a general-purpose
If you use a general-purpose micromechancs code like VAMUCH , you should have not problem to get all the 3D properties within one analysis over the unit cell.