Representative Volume Element Calculations under Constant Stress Triaxiality, Lode Parameter, and Shear Ratio

Recent experiments showed that the Lode parameter, which distinguishes between axisymmetric and shear dominated stress states, has a profound effect on material ductility, especially at low stress triaxiality. Consequently, the theoretical framework for void growth and coalescence is currently being revisited, which often involve performing representative volume element (RVE) calculations. The present study investigates an RVE composed of a cubic unit cell containing a spherical void at its center.