Ecoflex polymer : Comprehensive experimental study and constitutive modelling

We have published two papers on Ecoflex, a popular silicone polymer in recent days. The polymer is largely temperature- and strain rate-insensitive. It comes up with several Shore Hardnesses. We characterize five Shores and develop a novel Shore-dependent modelling framework

Mechanics of Materials >> https://www.sciencedirect.com/science/article/pii/S016766362030020X

Work of adhesion/separation between soft elastomers of different mixing ratios

Adhesion between soft matter is a universal mechanical problem in bio-engineering and bio-integration. The Johnson–Kendall–Roberts (JKR) method is widely used to measure the work of adhesion and work of separation between soft materials.