Electroelasticity of polymer networks

This work introduces a new microscopically-motivated model for the electromechanical response of elastomers:

http://ac.els-cdn.com/S0022509615303525/1-s2.0-S0022509615303525-main.pdf?_tid=1db1e302-202a-11e6-8a60-00000aacb361&acdnat=1463927774_d9ad1fa74b5b42fafcb28a8b6b2c9b60

The merit of this novel model is demonstrated in the following paper