Effects of SiC, SiO2and CNTs nanoadditives on the properties of porous alumina-zirconia ceramics produced by a hybrid freeze casting-space holder method

Highly porous alumina-zirconia ceramics were produced by adding space-holder materials during freeze casting. To increase the strength of porous ceramics, different amounts of nanoadditives (silicon carbide-SiC, silica-SiO2, and multi-wall carbon nanotubes-CNTs) were added. Space-holder materials were removed by preheating, and solid samples were produced by sintering. Up to 68% porosity was achieved when 40% space-holder was added to the solid load of slurry. Wall thicknesses between pores were more uniform and thinner when nanoadditives were added.