Helices are ubiquitous building blocks in natural and engineered systems. Previous studies showed that helical ribbon morphology can result from anisotropic driving forces and geometric misorientation between the principal axes of the driving forces and the geometric axes. However, helical ribbon shapes induced by elastic modulus anisotropy have not been systematically examined even though most natural and engineered structures are made of composite materials with anisotropic mechanical properties.