A note on the pull-off force for a pattern of contacts distributed over a halfspace

ArticleinMeccanica · March 2017 --- We found a very simple formula for pull-off force for a pattern of contacts distributed over an halfspace which could be very useful in predicting the adhesive propreties of structured surfaces, as bioinspired surfaces.  