Compressible, Dense, Three-Dimensional Holey Graphene Monolithic Architecture

We demonstrated outstanding compressibility of holey graphene nanosheets, which is impossible for pristine graphene. Holey graphene powder can be easily compressed into dense and strong monoliths with different shapes at room temperature without using any solvents or binders. 

ACS Nano, Article ASAP,