Investigating phase formations in cast AlFeCoNiCu high entropy alloys by combination of computational modeling and experiments

Selection and thermal stability of phases are important in design of high entropy alloys (HEA). In this study, phase formations in cast AlFeCoNiCu HEA were investigated. Ab-initio molecular dynamics (AIMD) simulations were used to determine crystal structures of phases at different temperatures in equiatomic composition of AlFeCoNiCu. The AIMD results showed a possible coexistence of a face-centered cubic (fcc) phase and a bodycentered cubic (bcc) phase at the room temperature and indicated stabilization of a single fcc phase above 1070 K at the equiatomic composition of AlFeCoNiCu.