Harnessing Surface Wrinkling-Cracking Patterns for Tunable Optical Transmittance

Optical devices and systems with tunable optical transmittance have recently attracted great interest due to their wide range of applications. However, the reported methods of realizing tunable optical transmittance still suffer from complex fabrication processes, high cost, unstable materials or low tuning range. In this study, we report a simple, cheap, and highly effective approach to achieve large tuning range of optical transmittance through harnessing surface wrinkling-cracking patterns on PDMS films.