Mechanics of an elastic solid reinforced with bidirectional fiber in finite plane elastostatics

A continuum-based model is presented for the mechanics of bidirectional composites subjected to finite plane deformations. This is framed in the development of a constitutive relation within which the constraint of material incompressibility is augmented. The elastic resistance of the fibers is accounted for directly via the computation of variational derivatives along the lengths of bidirectional fibers. The equilibrium equation and necessary boundary conditions are derived by virtue of the principles of virtual work statement.