Aging-dependent strain localization in amorphous glassy polymers: from necking to shear banding

This study investigates the influence of physical aging on the deformation behaviors of poly(ethylene terephthalate)-glycol. The polymers are subjected to a quenched and an annealed heat treatment, followed by deformation in tension. The digital image correlation (DIC) is used to capture the surface strain. The DIC results show that the deformation localization occurs in the post-yield strain softening region. The quenched and annealed polymers exhibit different localization types, representing as necking for quenched polymers and shear banding for annealed polymers.