Dear Colleagues,

Please see the link for a recent article published in Scripta Materialia. In this article, active cross-slip behavior of screw <c + a> dislocations in Mg is observed, and the plausibility of <c + a> dislocation slip on new planes {-12-11} that have hitherto not been considered possible, is shown for the first time.