Elaborating the controversy on the contribution of the surface stress in silicon nanowires

A link between the local surface stress at the atomic scale to the overall behavior of the continuum system indicates a twist deformation at the free end of silicon nano-cantilever. The importance of size and crystal orientation is demonstrated (for more details of the project see:https://www.researchgate.net/publication/327768951_Surface_Stress_Effect...).