Submitted by MichelleLOyen on Tue, 2008-05-06 14:46.Just published in this month's Journal of Materials Research--a study on poroelastic nanoindentation characterization for hydrated bone samples. Poroelastic problems are notoriously difficult to incorporate into routine materials characterization due to the paucity of problems with closed-form solutions. However, in some cases, a master-curve does exist and parameter identification can be accomplished without requiring inverse finite element analysis and optimization for every condition. The abstract follows, linked from here .
Poroelastic nanoindentation responses of hydrated bone, J. Mater. Res. 23 (2008) 1307.
»