Experimental temperature field at the crack tip in a natural rubber

Dear colleagues, this is a paper on the experimental determination of temperature field at the crack tip in a natural rubber using a motion compensation technique. The contribution of the non-uniformity of the IR detectors and the Narcissus effect is taking into account to determine the temperature field.

JB LE CAM