Hi,

 

I have developed a FORTRAN code to simulate the molding process of glass to make lenses. Hence, it involves a contact analysis between the glass and molds. The contact is modeled using the master and slave node concept and the mold is assumed to be rigid. For the application of this code, we are looking at highly precise dimensions to capture the curve of the mold on the glass after molding.