Stress-induced phase transformation and pseudo-elastic/pseudo-plastic recovery in intermetallic Ni–Al nanowires
Submitted by Vijay Kumar Sutrakar on Sun, 2009-07-05 08:04.Dear friends,
I want to share our recent research work on NiAl nanowire, which is published in Nanotechnology, IOP publishing. The abstract of the paper is given below. Further details can be found at " 2009 Nanotechnology 20 295705 (9pp) doi: 10.1088/0957-4484/20/29/295705"
»