Mechanics of a process to assemble microspheres on a patterned electrode
Submitted by Ting Zhu on Wed, 2006-12-20 17:26.T. Zhu, Z. Suo, A. Winkleman, G. M. Whitesides, Applied Physics Letters, 88, 144101, (2006)
A process has been demonstrated recently to assemble microspheres on a patterned electrode under the influence of an applied voltage. Here we examine the mechanics of this process, and describe both the conditions under which excess microspheres jump off the electrode when the voltage is applied, and the forces that attract the remaining microspheres to the desired positions. A quantitative mechanistic understanding of this process rationalizes experimental observations, provides scaling relations, and suggests modifications of the process.
»
- Ting Zhu's blog
- Login or register to post comments
- 1222 reads


Recent comments
11 hours 27 min ago
12 hours 54 min ago
15 hours 33 min ago
1 day 5 hours ago
1 day 6 hours ago
1 day 7 hours ago
1 day 8 hours ago
1 day 10 hours ago
1 day 15 hours ago
1 day 17 hours ago