Machining simulation
AISI 4150 or DIN 50CrMo4 Steel Flow Stress Curve Data for Machining Simulation
Submitted by ashwin.devotta on Sun, 2010-03-21 21:53.Hi All,
I am into machining simulation of 50CrMo4 Steel in DEFORM 3D and I need the flow stress curve data for various temperature and various strain rates. I have searched in as many journals as possible, but in vain. It would be of immense help if some one could share the material model data with me.
Thanking you in advance
With Best Regards
Ashwin Devotta
ashwin.devotta@gmail.com
»