Constitutive modeling of tension-torsion coupling and tension-compression asymmetry in NiTi shape memory alloys

A 3D constitutive model is proposed and verified with experimental data. Tension-torsion coupling effect and tension-compression asymmetry effect is investigate for tube shape memory alloy.