In this review of particularly readworthy papers in EFM, I have selected a paper about the tearing of large ductile plates, namely:
”Cohesive zone modeling and calibration for mode I tearing of large ductile plates” by P.B. Woelke, M.D. Shields, J.W. Hutchinson, Engineering Fracture Mechanics, 147 (2015) 293-305.