An introductory paper on thermal combinatorial analysis of nano-scale materials
Submitted by Patrick J McCluskey on Tue, 2007-02-06 19:30.If you are interested in nano-calorimetry or combinatorial analysis, you might also find the following paper interesting. It was published as part of the MRS spring ‘06 meeting proceedings (http://www.mrs.org/s_mrs/sec_subscribe.asp?CID=6447&DID=175796&action=de...). This paper describes the parallel nano-differential scanning calorimeter (PnDSC), a new device for measuring the thermal properties of nano-scale material systems using a combinatorial approach.
»