Graphene and Carbon Nanotubes are self-stressed

In the attached paper we have shown that graphene and carbon nanotubes are in a self-stress state in their natural equilibrium state, that is, the state prior to the application of external loads. We have identified different sources of self-stresses and accurately evaluated them; we have shown that they are by no means negligible with respect to load-related nanostresses.