Anisotropic yield, plastic spin, and dislocation mechanics

(This paper is to appear in the IUTAM Procedia on "Linking scales  in computations: from microstructure to macro-scale properties," edited by Oana Cazacu)

Amit Acharya, S. Jonathan Chapman