I would like to share our recent research work on FCC metallic nanowires, which is published in Journal of Physics : Condensed Matters (IOP) . The abstract of the paper is given below. Further details can be found at
Vijay Kumar Sutrakar et al 2012 J. Phys.: Condens. Matter24 015401