User login

You are here

X-ray microtomography (XMT)

Post Doctoral Research Position in Experimental Biomechanics at the University of Southampton, UK

The Bioengineering Science Research Group at the University of Southampton invites applications for an 18 month post-doctoral position investigating the mechanical performance of unicondylar knee arthroplasty (UKA). 

Research Associate in 4D Image based quantification and simulation

An excellent opportunity to work in a world leading team with privileged access to facilities that most researchers can only dream about.

Newton International Fellowships

"The Newton International Fellowship scheme will select the very best early stage post-doctoral researchers from all over the world, and offer support for two years at UK research institutions."

http://www.newtonfellowships.org

If you are interested in applying for a Newton Fellowship at the University of Manchester, meet the criteria specified on the url above, and have a background in:

FE mesh of particulate-reinforced metal matrix composite

Background of Study

  • Based on X-ray tomography (XMT)
  • Multi-part FEA model
  • Scan to mesh in 10 minutes

Aluminum-based particulate-reinforced metal matrix composites (PMMCs) frequently have a heterogeneous distribution of reinforcement particles whether produced by a powder or liquid processing route. The applicability of X-ray microtomography (XMT) for the characterization of this heterogeneity and its influence on final properties was investigated, for the case of a powder blended and extruded AA2124 matrix with Ni particulate. Simpleware software was used to quantify the embedded Ni particle size distribution and the extent and texture of clusters formed.