Thermodynamic model for strain-induced crystallization in rubber - Eccomas

Natural rubber (NR) is known to crystallize under strain (SIC) so that NR samples subjected to loading-unloading cycles exhibit hysteresis. A brief review of the numerous experiments conducted on this material is given. Detailed information on the microstructure is therefore available, particularly simultaneous measurements of stress versus elongation and