Mogadalai Gururajan's picture

Elastic stress driven rafting

During solid-solid phase transformations elastic stresses arise due to a difference in lattice parameters between the constituent phases. These stresses have a strong influence on the resultant microstructure and its evolution; more specifically, if there be externally applied stresses, the interaction between the applied and the transformation stresses can lead to rafting.