3-D Microstructure Reconstruction of Polymer Nano-Composite using FIB-SEM and Statistical Correlation Function

 http://www.sciencedirect.com/science/article/pii/S0266353813001012?np=y
Abstract

3-D
reconstruction of Halloysite nanotube (HNT) polypropylene composite has
been performed using two different methods. In the first method,
several slices of the composite material were obtained using focused ion
beam (FIB), and scanning electron microscopy (SEM). A representative
volume element (RVE) of the real material’s micro/nanostructures was