Mixed assumed-strain finite element model for laminates

Fibre-reinforced plates and shells are finding an increasing interest in engineering applications; in most cases dynamic phenomena need to be taken into account. Consequently, effective and robust computational tools are sought in order to provide reliable results for the analysis of such structural models. In this paper the mixed assumed-strain laminated plate element, previously used for static analyses, has been extended to the dynamic realm. This model is derived within the framework of the so-called First-order Shear Deformation Theory (FSDT).

Laminated composite smart stiffined plate

I am working on topic ' Finite Element Analysis of laminated composite smart stiffened plate'. I am not getting proper proper mathematical formulation for using in coding for MATLAB program.