Effect of fiber arrangement on mechanical properties of short fiber reinforced composites

2-D "tension-shear chain" model (Ref.1-3) is well known successfully capturing the basic mechanical features of staggered structures in shell-like biomaterials. Our recent paper appeared in Comp. Sci. Tech. developed a three-dimensional (3D) "tension-shear chain" theoretical model to predict the mechanical properties of unidirectional short fiber reinforced composites, and especially to investigate the distribution effect of short fibers.