Development of advanced materials for high-end applications is driven by the increasing understanding of the dynamics and properties of defect microstructures, leading to the ability to synthesize and control materials microstructures to meet specific application demands. Dislocation motion is the fundamental physical mechanism of the plastic deformation process in crystalline materials.